Monel K-500 Casting Parts
video

Monel K-500 Casting Parts

Material:Superalloy material ,Inconel、Nimonic、Incoloy、Hastelloy、Nickel、Monel、Stellite
Tolerance:CNC Machining ±0.004mm/Casting ±0.1mm
Service:Drawing Custom
Surface Treatment:Polishing,Electro-plating, Power coating,etc.according to your requirements.
Place of Origin:Qingdao, Shandong, China
Send Inquiry
Product Introduction

Product name: Customized Stellite superalloy casting cnc-machining Parts

product-1-1

Material:
Hastelloy: B B2X C276 C22 C-4 C2000 N G-3 G-30 G-35
Inconel: 625 600 601 800 718 725 926 X750
Incoloy: 800H 800HT 825 901 925
Monel: 400/M-400, K500/K-500

Stellite:Stellite1,3,4,6,12,19,20,21,25,31,190,250,694,700
Superalloy: GH 605 617 1140 2132 2909 3030 3039 3044 3128 3230 4145 4169 4202 4738 5188
Nimonic: Nimonic 75/80A/90/A263

 

Chemical composition of Monel 400:

Nickel: 63

Copper: 28-34

Iron: 2.5

Carbon: 0.3

Manganese: 2

Silicon: 0.5

Sulfur: 0.024

Physical properties of Monel 400:

Density: 8.83 g/cm3

Melting point: 1300-1390 ℃

Mechanical properties of Monel 400 alloy at room temperature:

Tensile strength Rm N/mm2: 480

Yield strength RP0.2N/mm2: 170

Elongation A5%: 35

This alloy has the following characteristics: Monel400 is a corrosion-resistant alloy with the widest usage and best application. This alloy has excellent corrosion resistance in fluorine and hot concentrated alkali solutions. It is also resistant to corrosion by neutral solutions, water, seawater, atmosphere, organic compounds, etc. An important feature of this alloy is that it generally does not produce stress corrosion cracks and has good cutting performance.

Metallographic structure of Monel 400: The organization of Monel 400 alloy is a high-strength single-phase solid solution.

Corrosion resistance of Monel 400: Monel 400 alloy has excellent corrosion resistance in fluorine gas, LIU acid, and their derivatives. At the same time, it is more corrosion-resistant than copper-based alloys in seawater. Acid medium: Monel 400 is corrosion-resistant in LIU acid with a concentration of less than 85%. Monel 400 is one of the very few important materials that can resist acid.

Water corrosion: Monel 400 alloy has good corrosion resistance in most water corrosion conditions, and pitting corrosion and stress corrosion are rarely found, and the corrosion rate is less than 0.025mm/a.

High temperature corrosion: The temperature of continuous operation of Monel 400 in air is generally around 600℃, and the corrosion rate in high-temperature steam is less than 0.026mm/a.

Ammonia: Due to the high nickel content of Monel 400 alloy, it can resist corrosion under anhydrous ammonia and ammoniation conditions below 585°C.

Application scope of Monel 400 Application fields are:Pump shaft,fastener,Ship propeller shaft,Oil drilling tool,appearance,spring

 

Monel® K-500 

Application field:
Due to its excellent corrosion resistance and high temperature strength, Monel K-500 alloy is widely used in the manufacture of equipment in the field of Marine engineering and petrochemical industry. For example, it can be used to manufacture thrusters, pumps, valves and piping systems for ships. In addition, Monel K-500 alloys can also be used in the manufacture of chemical processing equipment, nuclear energy equipment and aerospace components.
Comparison with other metal materials:
Monel K-500 alloy has higher corrosion resistance and high temperature strength compared to other metal materials. For example, compared with stainless steel, Monel K-500 alloy has better corrosion resistance and high temperature strength, which can be used in harsher environments. In addition, Monel K-500 alloy has better processing and weldability than stainless steel.
In short, Monel K-500 alloy is a high-performance metal material with excellent corrosion resistance and high temperature strength, which is widely used in the manufacture of equipment in the field of Marine engineering and petrochemical industry. Compared with other metal materials, Monel K-500 alloy has higher performance and use value.

 

H0dda3decb58f4a0b9b688285ec7e32e2m

H3d74cd8db3024967a4fbf78ceeb912fbB

H25b5f70412db48e5991ff6b5f624c8292

HTB184VQdjrguuRjy0Feq6xcbFXaW

Company Introduction

OBT is a professional machining equipment factory for superalloy casting, forging and CNC machining.We can not only produce materials required by customers but also high-end complex castings made of titanium alloys, high-temperature alloys(such as Inconnel,Hastelloy,Nimonic,Nickel), stainless steel ,brass and other materials. We also support customized materials. And can flexibly adopt die casting, Precision casting, sand casting,CNC machining and other processes.

As a company with rich superalloy and casting, forging manufacturing experience, we have advanced production equipment such as Vacuum Casting Furnace, Creep Endurance Tester,Steam Dewaxing Furmnace, Five-Axis Machining Center, Computer Numerical Control (CNC) Machine Tool, Tensile Testing Machine,Coordinate Measuring Machine (CMM) SPECTRO Spectrometer, etc. This allows us to control the precision within 0. 004mm-0.01mm.

We sincerely look forward to cooperating with you!

product-1-1

product-1-1
product-1-1

Hot Tags: Monel K-500 Casting Parts, China Monel K-500 Casting Parts manufacturers, suppliers, factory

Send Inquiry

whatsapp

Phone

E-mail

Inquiry