Kovar Alloy Strip
Melting point: 1450℃
Density: 8.4 g/m3 Elastic modulus: 138Gpa
Curie point: 430°C
Specific heat capacity: 649 J/(kg·℃)
KOVAR
Kovar alloy has a linear expansion coefficient similar to that of borosilicate hard glass at 20-450 ° C, a higher Curie point, and good low-temperature structural stability. The oxide film of the alloy is dense and can be well wetted by glass. And it does not interact with mercury, so it is suitable for use in instruments containing mercury discharge. It is the main sealing structure material of electric vacuum devices.
Similar Grades
United States: Kovar
United Kingdom: NiloK
Germany: Vacon12
Executive Standard
ASTM F15
standard as required
Typical values( %)
|
Ni |
Co |
Fe |
C |
Si |
Mn |
P |
S |
|
28.5 -29.5 |
16.8 -17.8 |
Remain |
≤0.03 |
≤0.30 |
≤0.50 |
≤0.015 |
≤0.01 |
Mechanical Properties (Annealed State)
|
Temperature ℃ |
Yield Strength R p0.2/MPa |
Tensile Strength R m/ MPa |
Elongation δ5 /% |
|
23 |
520 |
330 |
30 |
Application Field
● Used in electric vacuum components such as launch tubes
● Oscillating tube
● Pilot tube
● Magnetron
● Transistor
● Sealed plug
● Relay
● Outlet wires of integrated circuits
● Chassis
● Shell
● Glass sealing of brackets, etc.
Hot Tags: kovar alloy strip, China kovar alloy strip manufacturers, suppliers, factory, 4J36 Tube, Hastelloy B 3 Forgings, Hastelloy B 2 Strip, Hastelloy X Tube, Inconel X 750 Tube, Hastelloy C 276 Strip