Alloy X-750 Bolts
Density: 8.3 g/cm3
Melting point: 1395°C-13425°C
Resistivity: 1.22 x 10-6Ω
Alloy X-750 has good corrosion resistance and oxidation resistance below 980°C, high strength below 800°C, good relaxation resistance below 540°C, and good formability and welding performance. Excellent mechanical properties in low temperature environment.
Similar Grades
United States InconelX-750, UNS N07750
Germany W.Nr.2.4669, NiCr15Fe7TiAl
French NC15Tn
Chemical Composition
|
Composition |
Mix |
Max |
|
C |
|
0.08 |
|
Cr |
14.0 |
17.0 |
|
Ni+Co |
70.0 |
|
|
Al |
0.4 |
1.0 |
|
Ti |
2.25 |
2.75 |
|
Fe |
5.0 |
9.0 |
|
Nb+Ta |
0.7 |
1.2 |
|
Co |
|
1.0 |
|
Si |
|
0.5 |
|
Mn |
|
1.0 |
|
P |
|
0.015 |
|
S |
|
0.010 |
|
Cu |
|
0.5 |
Mechanical Properties (Room Temperature)
|
Variety |
σЬ / MPa |
σ0..2 / MPa |
δ5 / % |
|
Wire |
1110 |
- |
- |
|
Stripe |
≤930 |
- |
≥18 |
|
Plate |
≤930 |
≤515 |
≥30 |
|
Tube |
≤965 |
≤550 |
≥35 |
Thermal Conductivity
|
Θ/℃ |
λ/(W/(m·℃) |
|
50 |
14.7 |
|
100 |
15.9 |
|
300 |
20.1 |
|
500 |
25.1 |
|
900 |
37.3 |
Linear Expansion Coefficient
|
Θ/℃ |
α/10-6℃-1 |
|
20-200 |
13.1 |
|
20-300 |
13.5 |
|
20-400 |
14.1 |
|
20-500 |
14.4 |
|
20-600 |
15.0 |
|
20-700 |
15.6 |
|
20-800 |
16.2 |
Formability
1. The temperature range of thermal processing is 980-1200℃, and the cooling method can be water quenching or rapid air cooling;
2.The heating temperature of steel ingot forging can be 1200°C. In order to obtain good structure and properties of the final forging or bar, the subsequent forging heating temperature should be carried out at a correspondingly lower temperature. The final forging temperature should not be lower than 950°C. The alloy should be solution treated after the severe forming process.
Hot Tags: alloy x-750 bolts, China alloy x-750 bolts manufacturers, suppliers, factory, Hastelloy X Forging Parts, Inconel X 750 Forgings, 1J22 Casting Parts, Hastelloy X Bolts, Co27 Forging Parts, A 286 Threaded Trunnion