Stellite Superalloy Casting CNC Machining Parts
Tolerance:CNC Machining ±0.004mm/Casting ±0.1mm
Service:Drawing Custom
Surface Treatment:Polishing,Electro-plating, Power coating,etc.according to your requirements.
Place of Origin:Qingdao, Shandong, China
Product name: Customized Stellite superalloy casting cnc-machining Parts





| Stellite 3 Alloy | |||||||
| Co | Cr | W | C | Others | Hardness | Density | Melting Range |
| Base | 30.5 | 12.5 | 2.3 | Ni, Fe, Si | 48-63 HRC | 8.69 g/cm3 | 1250-1290ºC |
| 0.314 lb/in3 | 2280-2355ºF | ||||||
| Stellite alloy 1 | |||||||
| Co | Cr | W | C | Others | Hardness | Density | Melting Range |
| Base | 28-32 | 11月13日 | 2.0-3.0 | Ni, Fe, Si, Mn, Mo | 50-58 HRC | 8.69 g/cm3 | 1248-1290ºC |
| 550-720 HV | 0.314 lb/in3 | 2278-2355ºF | |||||
| Stellite 4 Alloy | |||||||
| Co | Cr | W | C | Others | Hardness | Density | Melting Range |
| Base | 30 | 14 | 1 | Mn, Fe, Si, Ni | 45-49 HRC | 8.61 g/cm3 | 1340-1395ºC |
| 0.311 lb/in3 | 2245-2545ºF | ||||||
| Stellite 6 Alloy | |||||||
| Co | Cr | W | C | Others | Hardness | Density | Melting Range |
| Base | 27-32 | 3月6日 | 0.9-1.4 | Ni, Fe, Si, Mn, Mo | 36-45 HRC | 8.44 g/cm3 | 1250-1360ºC |
| 380-490 HV | 0.305 lb/in3 | 2282-2480ºF | |||||
| Stellite 6 Alloy | |||||||
| Co | Cr | W | C | Others | Hardness | Density | Melting Range |
| Base | 27-32 | 7.5-9.5 | 1.4-2.0 | Ni, Fe, Si, Mn | 45-51 HRC | 8.53 g/cm3 | 1225-1280ºC |
| 435-590 HV | 0.308 lb/in3 | 2240-2335ºF | |||||
Features:Corrosion resistance Stellite 21 alloy shows good corrosion resistance, can resist acid, alkali, salt water and other corrosive media corrosion. This makes Stellite 21 widely used in the chemical, oil and gas industries.
- High temperature stability: Stellite 21 alloy can maintain its strength and stability in high temperature environment, and has good high temperature performance. Suitable for aerospace, energy, high temperature technology and other applications requiring high temperature wear.
- Corrosion resistance: Stellite 21 exhibits excellent corrosion resistance and can resist a variety of corrosive media, including acids, alkalis and brine.
- Oxidation resistance: Stellite 21 alloy resists the effects of oxidation and thermal corrosion at high temperatures, maintaining its properties and stability.Magnetic stellite 21 is usually non-magnetic and has low permeability.
- Weldability: Stellite 21 alloy has good weldability and can be connected with other metal materials, increasing its flexibility and diversity of applications.
Application field:
- Oil and gas industry: Stellite 21 is commonly used in the manufacture of wear and corrosion resistant parts such as valves, seals, valve stems, pump housings, wellhead equipment, etc., to cope with extreme working conditions and corrosive media.
- Chemical industry: Stellite 21 is widely used in chemical equipment and pipeline systems due to its excellent corrosion resistance, which is used to manufacture valves, pumps, pipe joints and other components to withstand the corrosion of acid and alkali media and work under high temperature and pressure conditions.
- Aerospace industry:Stellite 21 can be used to manufacture aeroengine components such as turbine blades, nozzles and combustion chamber components, providing high temperature and wear resistance.
- Energy industry :Stellite 21 alloy is commonly used in power plant mill components, boiler nozzles and grinding rolls to resist the wear of pulverized coal and the effects of high temperature environments.
- Other fields: Stellite 21 alloy can also be used in pump parts, chemical reactors, bearings, cutting tools, etc., providing solutions with high wear and corrosion resistance.
During the quotation stage, our professional engineers participate in the research process, judge the process according to customer's requirement, Before sample production, a review meeting is held to study key technology points based on customer requirements.
In the mass production stage, based on mature processes, ensure long-term stable quality.